A tub of wood filler costs less than lunch, and the wrong one still ruins a weekend. Some sand like chalk. Others stay rubbery, reject stain, or pop out of a deck board by spring. This guide sorts the options by the job at hand, with real Canadian prices and metric fill depths. More from us: Wood Chipper Buying Guide for Canada.
Short answer: Buy a water-based latex product for indoor trim and furniture, because it sands easily and takes paint well. Choose a solvent-based or epoxy formula for outdoor use, where moisture and movement break cheaper products apart. Putty is different again. Putty never hardens, so keep that one for finished surfaces and small dings.
Key takeaways
- Latex products are the default for indoor trim, doors, and furniture, at roughly CAD 15 for 170 g.
- Build deep repairs in layers of about 3 mm. One thick 6 mm slug may need 36 hours before it is ready to be sanded.
- Most tubs want a minimum working temperature above 4 degrees Celsius, so an unheated garage in a Canadian winter is out.
- Stainable does not mean invisible. Test on a scrap first.
- A large tub costs close to half as much per millilitre as the little tube beside it.
Types at a glance
The wood filler aisle looks like five versions of one product. It isn’t. Each row below behaves differently once it dries, which determines whether your repair survives.
| Type | Best for | Sands? | Takes stain? | Typical size and price |
|---|---|---|---|---|
| Water-based latex | Indoor trim, nail holes, furniture | Yes, easily | Fair, test it | 170 g, about CAD 15 |
| Solvent-based | Doors, sills, repairs that take screws | Yes, fast | Good | 473 mL, about CAD 22 |
| Two-part epoxy | Rotted or structural exterior wood | Yes, with effort | Poor; paint it | Kits from about CAD 30 |
| Powdered; mix with water | Deep fills and colour matching | Yes | Good | 150 g, about CAD 17 |
| Wood putty, non-hardening | Finished trim, floors, small dings | No | Pre-tinted only | 106 g, about CAD 11 |
What wood filler actually is

Nearly every tub holds two things: ground wood fibre or mineral powder, and a binder that sets around it. The binder is what changes from product to product. Water-based versions are made with a latex binder; they dry as the water leaves, clean up with a damp cloth, and barely smell.
Solvent-based formulas set harder and faster, and they smell like it, so open a window. Two-part epoxy sits at the far end of the range. You mix a resin with a hardener, and the result bonds to the sound fibre rather than just sitting in the hole. It is the only choice that rebuilds a missing corner of a windowsill and withstands freeze-thaw cycles.
Filler or putty? Check whether the finish is already on
This is the question that sends people back to the store. The two products sit side by side on the shelf and behave nothing alike on the wood.
A hardening compound belongs on bare wood, before any finish. Once dry, it is solid, sands flush, and accepts paint or stain. Putty is an oil- or plastic-based paste that remains soft indefinitely. That softness is the point, because it flexes over a floorboard rather than cracking, and it arrives pre-tinted to match common wood tones.
So patch bare pine trim with the hardening kind before you paint. Hide a nail hole in a stained oak stair tread with putty after the finish is on. Our trim and flooring renovation guides cover the order of operations when working through a whole room.
How to apply it without leaving a visible patch

- Clean the repair. Scrape out any loose fibre, vacuum up the dust, and let the damp wood dry fully first.
- Overfill slightly. The patch shrinks as it dries, and a proud mound sands flat in seconds. A sunken one means a second round.
- Press the material in with a flexible putty knife, working across the hole rather than along it. That forces it into the void instead of skimming the surface.
- Layer anything deeper than about 3 mm, letting each layer dry before you add the next. Cracks and open gaps in a joint want the same treatment.
- Sand with 120 grit, then 180 or 220. Feather the edge into the surrounding wood so no ridge catches the light.
- Vacuum the dust, then prime, paint, or seal within a day.
Two habits separate a clean job from an obvious one: overfilling and sanding with a block rather than bare fingertips. Fingers follow the dip and leave a shallow crater you only notice under paint.
Dry time, fill depth, and cold garages
Manufacturer sheets are worth reading, and the Canadian ones are stricter than the marketing copy. DAP’s Wood Pro data sheet for Canada gives roughly 3 to 6 hours before sanding on a shallow fill up to 3 mm. Go to 6 mm or deeper, and the same sheet asks for about 36 hours. Dry time scales sharply with depth, which is exactly why thin layers beat one thick pour.
Most guides quote depths in inches only. In millimetres, the practical ceiling for a single pass is around 3 mm. Anything past 10 mm wide is better closed with a glued sliver of matching wood, then patched at the seam.
Temperature matters as much as depth. That same sheet asks for the wood, the air, and the product all above 4 degrees Celsius. An unheated garage in Ottawa in February sits far below that, so the patch skins over, stays soft underneath, and crumbles the moment you sand it. Move the work indoors or heat the space for a day. A humid basement in July stretches the wait too, sometimes by half again.
Will it take stain? Run the scrap test.
“Stainable” on a label means the patch will accept pigment. That is not a promise the patch will disappear. Cured compound has no grain and a different density. Expect it to read a shade lighter or darker than the board beside it, and open-grain species like oak show that difference most.
Test before you commit. Fill a hole in a scrap of the same species, sand it, and brush your stain across both. Five minutes tells you whether to carry on, tint the compound with a little stain before you pack it in, or switch to tinted putty applied after the finish. For colour and styling decisions around repaired pieces, our finished wood and furniture ideas are a useful next read.
Paint forgives far more. If the piece is heading for primer and two coats, almost anything in the aisle works, and the seam vanishes.
What it costs in Canada
Here is what we priced at Rona in August 2026. Canadian Tire and Home Depot Canada carry the same LePage and DAP lines within a dollar or two. Lee Valley stocks powdered and two-part options the big-box aisles skip. Our related guide, Self-Propelled Lawn Mower, goes further into this.
| Product | Size | Price | Unit cost |
|---|---|---|---|
| LePage solvent-free tube | 90 mL | CAD 7.49 | about CAD 0.08 per mL |
| LePage Plastic Wood tub | 473 mL | CAD 22.69 | about CAD 0.05 per mL |
| LePage Plastic Wood tub | 946 mL | CAD 38.69 | about CAD 0.04 per mL |
| DAP Wood Pro-X | 156 g | CAD 13.79 | about CAD 0.09 per g |
| DAP Wood Pro-X | 453 g | CAD 21.29 | about CAD 0.05 per g |
| Minwax wood putty | 106 g | CAD 10.59 | about CAD 0.10 per g |
The pattern is blunt. A small tube costs roughly twice as much per millilitre as the large tub. Value tips tend to favor the bigger container once you have more than a handful of holes. Buy the tube anyway if this is a one-off, because an opened tub skins over and dries out within a year or two.
Our verdict for three common jobs

Painted indoor trim: we recommend a 473 mL tub of water-based latex compound. Cheap, quick to sand, and paint covers every trace of it.
Stained furniture or a stair tread: tinted putty applied after the finish, or a powdered product you can tint yourself before packing it in. Both beat trying to stain a latex patch to match.
A rotted sill, post, or deck board: two-part epoxy, every time. It costs three times as much, takes an afternoon, and is the only repair still holding up on outdoor decks after two Canadian winters.
Your next step
Match the product to the surface, not to the price tag, and buy one small tube of putty alongside your tub so you are covered either way. Then start with the least visible repair in the room and work toward the one at eye level. Ready for the next project? Browse our home repair projects and tools for more weekend fixes.
Frequently asked questions
Some grades handle it. Look for “exterior” or “weatherproof” on the label, and coat the repair with paint or solid stain, because sunlight and rain break down an uncoated patch. For anything structural, skip straight to epoxy.
In thin layers, surprisingly deep. In one pass, keep it under 3 mm. A void wider than about 10 mm needs a wood shim first, then a patch over the seam.
Water-based products shrink a little as the water evaporates, which is why you overfill. Epoxy and solvent-based versions move far less.
Into soft latex, no. Into a solvent-based or epoxy repair, yes, within reason. For a hinge screw in a stripped door jamb, glue in a dowel instead.
No. Drywall spackling sands beautifully and fails on wood that moves or gets handled. Keep it on your walls.